Fatigue Behaviour of Case-Carburized and Chromium Nitride (CrN) PVD-Coated EN353, SAE8620 and 20MnCr5 Steels: A Systematic Review
DOI:
https://doi.org/10.14741/ijcet/v.16.4.3Keywords:
Case Carburizing, Chromium Nitride (CrN), Fractography, PVD Coating, Residual Stress, Rotating-Bending Fatigue, Surface EngineeringAbstract
Case-carburized low-alloy steels such as EN353, SAE8620 and 20MnCr5 are widely used in gears, shafts and transmission components because carburization combines a hard, wear-resistant surface with a tough core. Physical vapour deposition of chromium nitride (CrN) improves wear and corrosion resistance of such components, but its effect on fatigue behaviour is inconsistently reported: some studies find CrN delays crack initiation and improves fatigue life, while others report reduced endurance limits from coating defects, residual stresses or interfacial debonding. This paper presents a systematic review, following a pre-defined search and screening protocol, of fatigue fundamentals case-carburization metallurgy, PVD/CrN coating technology, and comparative fatigue and fractographic behaviour reported for carburized and CrN-coated steels. A quantitative data-extraction table supplements the qualitative synthesis, recording case depth, hardness, retained austenite, coating parameters and reported fatigue outcome for every study, noting unreported variables. The synthesis shows that almost no study evaluates more than one carburizing steel under identical conditions, that rotating-bending fatigue is under-studied relative to axial and rolling-contact loading, and that fractographic observations are rarely correlated quantitatively with fatigue-life data. These gaps motivate a systematic comparison of the three steels under identical CrN coating and rotating-bending conditions, combined with correlated SEM fractography.